Sep 01, 2016 3.2. Methods and procedures. A stainless steel bowl was loaded with 200 g Al and 4 vol.% of Al 2 O 3 powders with a ball-to-powder weight ratio of 5:1; meanwhile, to identify the effect of the nanoscale Al 2 O 3 reinforcements on the ball-milled composite powders, 200 g of Al without Al 2 O 3 was loaded into another stainless steel bowl. To prevent excessive cold-welding, 3 wt.% of stearic ...